E-82 Epoxy Ground Adjustment

PRODUCT DESCRIPTION

In order to close small holes and pores on uneven and rough surfaces, to cut off the moisture that may come from the floor, to prevent dusting,

It is a 2-component epoxy floor primer used on dry surfaces to increase the adhesion and adhesion of the surface.


SCOPE OF APPLICATION

It is a floor primer used to prevent dust on the floor on damp and dusty floors, to cut moisture and to provide adherence.


FEATURES

Epoxy, polyurea, polyurethane etc. It performs very well as a floor primer for floor coatings and adhesives.

It is a solvent free primer.

It prevents dusting and provides a hygienic environment.

It eliminates the adhesion and swelling problems (reaction deterioration) of the adhesive caused by the ground.

It has high bonding and holding strength.

It is resistant to water, humidity and heat after application.

It provides great convenience in cleaning the floor after priming.

It provides a bright and smooth floor appearance.

It is resistant to simple solvents and acids.

It can be applied to slightly damp surfaces.


Usage time (23°C, Pot Life):

60 minutes

Full drying mechanical strength time:

5 days

Drying time (at 25 °C):

≤24 hours


APPLICATION

The surface on which the primer will be applied should be clean, free from oil and dirt, especially dry, repaired surface.

Mixture

All of the hardener is poured into the main material and mixed until a homogeneous mixture is obtained without dragging air. In order to make sure that the mixture is fully made, put the ingredients in another container and mix again until you get a smooth mixture. Mixing should be done with an electric mixer, it is applied to the floor with the help of a brush or roller. Under normal conditions, curing is 2-3 hours and drying time is 24 hours. In hot environments, the time is shorter, and in cold environments, this time may be longer. In order to avoid the problem of unreacted resin that may remain on the surface of the container, pour it into a separate clean container after making the mixture, mix it again and use it. In applications below 5°C, carbonization problem may occur on the surface.

How Can We Help You ?

you can connect to our whatsapp support line for your questions.